Genuine Polyplast 30* Thread forming screw for Thermoplastic

Click Here for larger image
Series 20210 Type : 1445
Genuine Polyplast 30* Thread forming screw for Thermoplastic
close
Part No. Diam. d1Diam. d2Pitch pX maxX Min.Head dia. DHeight K maxminRadius rSlot width nt max/min  
Part No. Diam. d1Diam. d2Pitch pX maxX Min.Head dia. DHeight K maxminRadius rSlot width nt max/min  
 1445K22xL2.21.250.982.21.14.21.35/1.150.900.60.55/0.80request sample 
 1445K25xL2.51.401.122.51.34.21.35/1.150.900.60.55/0.80request sample 
 1445K30xL3.01.661.343.01.55.61.75/1.501.000.80.75/1.00request sample 
 1445K35xL3.51.911.573.51.86.01.75/1.501.000.80.75/1.00request sample 
 1445K40xL4.02.171.794.02.06.92.10/1.851.201.00.95/1.25request sample 
 1445K50xL5.02.682.245.02.58.22.45/2.151.301.21.15/1.50request sample 
 1445K60xL6.03.192.696.03.09.52.80/2.501.601.21.35/1.70request sample 
Substitute the length for the L In the part no. to specify the exact part required.
The 30 deg. Flank angle and recessed core diameter of these thread forming screws for plastic have been developed following theoretical appraisal, exhaustive calculations and final proof testing. The 30 deg. Flank angle produces low radial forces when engaging the plastic, therefore resulting in less radial stresses and tension. In other words the hoop stresses in the plastic bosses are less than those experienced with conventional screws. The recessed core geometry provides the ideal flow director for the displaced plastic, encouraging a uniform flow to fill the pitch of the screw without material jamming. This results in the maximum amount of plastic being engaged to provide higher sheer loads, due to the increased bearing depth of the thread. A combination of the above and the ease of penetration of the 30 deg. Flank angle through the material and the way in which the plastic flows, reduces the torque required to drive the screw in. This fact therefore increases the margin between drive torque and stripping torque which of course minimises the potential of stripping during installation. The optimum pitch and maximum fill features provided by the recessed core results in a large area of plastic to be sheered prior to screw failure in tension. This creates a high resistance to pullout loads.
Request information about:
Series: 20210 Type: 1445 Genuine Polyplast 30* Thread forming screw for Thermoplastic
Your Question
/Enquiry:
Your
email address